Finox 4332 AC is an electrode for joint welding of unalloyed and low-alloyed steels with high-alloyed steels, cast steel tpyes and for austenite-ferrite joints at working temperatures of up to 300 °C. It is suited for welding of buffering layers and platings with the first layer already being corrosion-resistant as well as for welding of transition zones on chromium-nickel-plated sheets.
DIN EN ISO 3581-A | E 23 12 L R 32 |
AWS A 5.4 | E 309 L-16 |
Material no. | 1.4332 |
Type of current | AC DC plus pole |
|||||
Diameter | 2.5 mm 3.25 mm 4.0 mm |
|||||
Weld Metal Composition | C | Si | Mn | Cr | Ni | Structure |
0.02 % | 0.9 % | 0.7 % | 23 % | 13 % | Austenite with approx. 15 % ferrite |